JIS G3462 STBA 26 Seamless Steel Pipe
JIS G3462 STBA 26 Heat Exchanger Tubes
JIS G3462 STBA 26 seamless steel pipe is a heat-resistant steel specified in the Japanese standard JIS G3462. JIS G3462 STBA 26 high temperature seamless steel pipe has high temperature resistance and mechanical properties, and can withstand high temperature and high pressure working environment.
JIS G3462 STBA 26 has a stable structure after high temperature aging, low thermal expansion coefficient and good thermal conductivity. Therefore, it is widely used in high temperature and high pressure equipment and systems such as boilers, internal and external heat exchangers.
STBA 26 Pipe Chemical Composition
|
C |
|||||||
|
STBA 26 |
Less than or equal to 0.15 |
0.3-0.6 |
0.03 |
0.03 |
0.2-1.0 |
8.0-10.0 |
0.9-1.1 |
STBA 26 Mechanical Properties
|
ReH/Rp0,2 N/mm² min |
|||
|
STBA 26 |
206 |
412 |
20 |
STBA26 high pressure alloy pipe

Gnee has 14 steel production lines, 10 processing equipment for processing, bending, painting, heat treatment, cutting, drilling, beveling, tempering, surface treatment, complete testing equipment and strong technical force. The annual production capacity is more than 60,000 tons.

1. How do we ensure quality?
There are always pre-production samples before mass production;
2. What can you buy from us?
3. Why should you buy from us instead of other suppliers?
The factory covers an area of nearly 60,000 square meters and has processing equipment such as large shears, circular shears, straighteners, annealing furnaces, and punching and shearing lines.
গরম ট্যাগ: jis g3462 stba 26 seamless steel pipe, China jis g3462 stba 26 seamless steel pipe manufacturers, suppliers, factory
তুমি এটাও পছন্দ করতে পারো
অনুসন্ধান পাঠান